physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Mold shrinkage rate | ISO 294-4 | 0.40-0.60 % |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.16 g/cm | |
melt mass-flow rate | ISO 1133 | 30.0 CM |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
yield stress | ISO 527-2 | 39.0 Mpa | |
Flexural modulus | ISO 178 | 2450 Mpa | |
bending strength | ISO 178 | 67.0 Mpa | |
Charpy Notched Impact Strength | ISO 179 | 5.00 KJ/m | |
ISO 179 | 15.0 KJ/m | ||
Rockwell hardness | ISO 2039-2 | 105 R scale | |
Tensile modulus | ISO 527-2 | 2300 Mpa |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | ISO 75-2/Af | 74.0 °C | |
Linear coefficient of thermal expansion | ISO 11359-2 | 0.000080 cm/cm/℃ | |
Flame retardancy | UL 94 | V-0 | |
UL 94 | 5VB | ||
UL 94 | 5VA |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.