SBS Taipol 4270 Taiwan Synthetic Rubber

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7920.948 g/cm³
melt mass-flow rateASTM D123816to25 g/10min
Bound styrene内部方法36.0to38.0 %
ash contentASTM D5667<0.10 %
gel content内部方法<0.10 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224086
optical performance Test ConditionTest MethodTest Result
Yellowness Index内部方法<4.0 YI
Supplementary InformationTest ConditionTest MethodTest Result
Volatile compounds内部方法<0.50 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.