Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.20到1.36 g/cm³ |
Water absorption rate | | ASTMD570 | 0.12到0.75 % |
Shrinkage rate | | ASTMD955 | 0.79到0.81 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 105到125 |
optical performance | Test Condition | Test Method | Test Result |
---|
transmissivity | | ASTMD1003 | 87.0到88.1 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 53.0到72.8 MPa |
elongation | | ASTMD638 | 2.5到82 % |
Flexural modulus | | ASTMD790 | 1100到2660 MPa |
bending strength | | ASTMD790 | 76.0到105 MPa |
compressive strength | | ASTMD695 | 76.0到86.0 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 43到450 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1.0E+14到2.1E+16 ohms·cm |
dielectric strength | | ASTMD149 | 24到39 kV/mm |
dielectric constant | | ASTMD150 | 2.60到3.77 |
Dissipation Factor | | ASTMD150 | 0.010到0.040 |
arc resistance | | ASTMD495 | 79.3到128 sec |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 6.0E-5到7.4E-5 cm/cm/°C |
| | ASTMD648 | 110到176 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.