Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:120 |
| | | 按重量计算的混合比:100 |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792,ASTMD1622 | 1.25 g/cm³ |
Shrinkage rate | | 内部方法 | 0.75 % |
Water absorption rate- | | 内部方法 | 0.10 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
HeatSag | | ASTMD3769 | 0.500 mm |
DartImpact | | 内部方法 | 801 J/m |
HeatSag | | ASTMD3769 | 4.50 mm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ASTMD790 | 2590 MPa |
Flexural modulus | | ASTMD790 | 1720 MPa |
Flexural modulus | | ASTMD790 | 1030 MPa |
elongation | | ASTMD638 | 15 % |
tensile strength | | ASTMD638 | 37.9 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD412 | 37.9 MPa |
elongation | | ASTMD412 | 15 % |
tear strength | | ASTMD624 | 123 kN/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 7.1E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.