PP Homopolymer Tisoplen® PPH UNR FR

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rate1.5 %
Water absorption rateISO 620.010 %
densityISO 11831.03 g/cm³
melt mass-flow rateISO 113320 g/10min
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 86868
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-0
Burning wire flammability indexIEC 60695-2-12960 °C
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldISO 527-225.0 MPa
tensile strength BreakISO 527-226.0 MPa
Tensile strainYieldISO 527-238 %
Tensile strainBreakISO 527-240 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/A4.0 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 2
Thermal performanceTest ConditionTest MethodTest Result
melting temperature165 °C
Heat distortion temperatureISO 75-2/Be120 °C
vicatISO 306/B120150 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.