Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | Yield | ISO 527-2 | 47.0 | Mpa |
| Tensile strain | Yield | ISO 527-2 | 4.5 | % |
| Break | ISO 527-2 | 50 | % | |
| Bending modulus | ISO 178 | 1900 | Mpa | |
| Charpy Notched Impact Strength | -40℃ | ISO 179 | 19 | kJ/m² |
| 23℃ | ISO 179 | 82 | kJ/m² | |
| -30℃ | ISO 179 | 无断裂 | ||
| 23℃ | ISO 179 | 无断裂 | ||
| Impact strength of cantilever beam gap | -30℃ | ISO 180 | 17 | kJ/m² |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | Across Flow: 23 to 55℃, 2.00 mm | ISO 11359-2 | 0.00012 | cm/cm/℃ |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 148 | °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 61.0 | °C | |
| Melting temperature | ISO 11357-3 | 262 | °C | |
| Linear coefficient of thermal expansion | Flow: 23 to 55℃, 2.00 mm | ISO 11359-2 | 0.00014 | cm/cm/℃ |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | TD: 2.00 mm | ISO 294-4 | 1.6-1.9 | % |
| MD: 2.00 mm | ISO 294-4 | 1.7-2.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.