impact performanceTest ConditionTest MethodTest ResultTest Unit
Charpy Notched Impact Strength0°CISO 179/1eA3.0kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA5.0kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A2.0kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A6.0kJ/m²
Charpy Notched Impact Strength-20°CISO 179/1eA2.5kJ/m²
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.6mmUL 94HB
Hot filament ignition temperature2.0mmIEC 60695-2-13650°C
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile modulus23°CISO 527-2/51300MPa
tensile strengthBreak,23°CISO 527-2/528.0MPa
Tensile strainYield,23°CISO 527-2/56.5%
Tensile strainBreak,23°CISO 527-2/550%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B88.0°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A51.0°C
Vicat softening temperature--ISO 306/A151°C
Vicat softening temperature--ISO 306/B67.0°C
Melting temperatureISO 11357165°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate230°C/2.16kgISO 113312g/10min
Shrinkage rateTD1.3%
Shrinkage rateMD1.3%
densityISO 11830.905g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.