TPU-Ester Elastollan® C70AW

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.15 g/cm³
melt mass-flow rateASTMD123810to30 g/10min
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224069
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusInjectionASTMD41211.0 MPa
Flexural modulusInjectionASTMD79013.1 MPa
ASTMD104440.0 mg
Abrasion-DINDIN5351620 mm³
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD41210.3 MPa
tensile strengthASTMD41227.6 MPa
elongationBreakASTMD412720 %
tear strengthASTMD62477.1 kN/m
compression setASTMD395B20 %
compression setASTMD395B45 %
Tensile stressASTMD4124.14 MPa
Thermal performanceTest ConditionTest MethodTest Result
SofteningPoint-DMA内部方法89 °C
Glass Transition Temperature内部方法-48.0 °C
vicatASTMD152567.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.