Share
Add to compare

PC NAXELL™ PC210HR MRC USA

Typical Applications:
Thin walled components
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:Thin walled components

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°C,3.20mmASTM D256590J/m
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating3.18mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
tensile strengthYield,23°C,3.18mmASTM D63862.0MPa
elongationBreak,23°C,3.18mmASTM D63850%
Bending modulus23°C,3.18mmASTM D7902270MPa
bending strength23°C,3.18mmASTM D79093.0MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,Unannealed,3.18mmASTM D648132°C
Hot deformation temperature1.8MPa,Unannealed,3.18mmASTM D648120°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate300°C/1.2kgASTM D123825g/10min
Shrinkage rateMD:3.18mmASTM D9550.50to0.70%
densityASTM D7921.19g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.