Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO 1183 | 0.922 g/cm³ |
melt mass-flow rate | | ISO 1133 | 0.27 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTM D2457 | >20 |
Haze ratio | | ASTM D1003 | <15 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | Compression Molded | ISO 527-2 | 240 MPa |
tensile strength | | ISO 527-2 | 10.0 MPa |
film | Test Condition | Test Method | Test Result |
---|
film thickness | | | 70 µm |
tensile strength | | ISO 527-3 | 24.0 MPa |
tensile strength | | ISO 527-3 | 18.0 MPa |
elongation | | ISO 527-3 | 320 % |
elongation | | ISO 527-3 | 550 % |
Dart impact | | ASTM D1709 | 200 g |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ASTM D1525 | 95.0 °C |
melting temperature | | ISO 11357-3 | 111 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.