physical property Test ConditionTest MethodTest Result
densityASTM D7920.980 g/cm³
Other performanceTest ConditionTest MethodTest Result
Ions内部方法7.00 ng/cm²
Ions内部方法5.00 ng/cm²
Ions内部方法16.0 ng/cm²
Ions内部方法53.00 ng/cm²
Analysis of evolved gases内部方法1.00 µg/g
Analysis of evolved gases内部方法<0.100 µg/g
Analysis of evolved gases内部方法7.00 µg/g
Ions内部方法<10.0 ng/cm²
nonvolatile content内部方法1.30 µg/cm²
Mechanical propertiesTest ConditionTest MethodTest Result
elongation at breakASTM D638200 %
Tensile modulusASTM D6381280 MPa
Flexural modulusASTM D7901280 MPa
Impact strength of cantilever beam gapASTM D256110 J/m
tensile strength ASTM D63828.0 MPa
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTM D2573E+10 Ω.cm
Surface ResistivityASTM D2578E+09 Ω.cm
static decay<1.0 sec
Surface ResistivityESDS11.118E+08 ohms
coefficient of friction内部方法10.0 V
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D64873.0 °C
Heat distortion temperatureASTM D64850.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.