PUR-TDI 107

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
STORAGE STABILITY6.0到8.0 min
stripping time2.0 min
STORAGE STABILITY25 min
Thermosetting mixed viscosityASTMD2393690 cP
stripping time6.0 min
physical property Test ConditionTest MethodTest Result
densityASTMD7921.21 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224089
Shore AASTMD224090
elastomerTest ConditionTest MethodTest Result
Basho elasticityASTMD263250 %
tensile strengthYieldASTMD41213.8 MPa
elongationBreakASTMD412600 %
Tensile stressASTMD4124.83 MPa
Tensile stressASTMD4127.58 MPa
Tensile stressASTMD4125.45 MPa
Tensile stressASTMD4128.27 MPa
tensile strengthYieldASTMD41214.5 MPa
elongationBreakASTMD412600 %
Basho elasticityASTMD263248 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.