PUR-Ester Interpol 47-5116/47-5205

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
960 min
Resin按重量计算的混合比:100
Hardener按重量计算的混合比:27
hardnessTest ConditionTest MethodTest Result
ASTMD224084
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTMD7903050 MPa
bending strengthYieldASTMD790131 MPa
Tensile modulusASTMD6382450 MPa
tensile strengthYieldASTMD63877.2 MPa
elongationYieldASTMD6388.4 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25645 J/m
Suspended wall beam without notch impact strengthASTMD256730 J/m
Thermal performanceTest ConditionTest MethodTest Result
ASTMD64887.8 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.