TPV Alloy Elastoprene 80A-4000

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7920.960 g/cm³
hardnessTest ConditionTest MethodTest Result
ASTMD224083
ASTMD224080
Supplementary InformationTest ConditionTest MethodTest Result
OzoneResistanceASTMD1149Excellent
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD4126.10 MPa
tensile strengthASTMD4129.30 MPa
elongationASTMD412430 %
tear strengthASTMD62448.0 kN/m
compression setASTMD39531 %
compression setASTMD39553 %
Thermal performanceTest ConditionTest MethodTest Result
melting temperature159 °C
brittle temperatureASTMD746-70.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.