physical property Test ConditionTest MethodTest Result
melt mass-flow rateJISK671920 g/10min
Water absorption rateASTM D570<0.010 %
optical performance Test ConditionTest MethodTest Result
transmissivityASTM D100392.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile strainISO 527-290 %
Flexural modulusISO 1782100 Mpa
Tensile modulusISO 527-22200 Mpa
tensile strength ISO 527-253.0 Mpa
Electrical performanceTest ConditionTest MethodTest Result
dielectric constantASTM D1502.30
Dissipation FactorASTM D150<1.0E-3
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureJISK7121102 °C
Linear coefficient of thermal expansionASTME8317E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.