Polyester EL740-H/A DSM Additive Manufacturing
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 10 | kJ/m² |
| -30°C | ISO 179/1eA | 4.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | IEC 60695-11-10,-20 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | 10%Strain | ISO 527-2 | 34.0 | MPa |
| Tensile modulus | ISO 527-2 | 1100 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.1E-04 | cm/cm/°C |
| MD | ISO 11359-2 | 1.1E-04 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 220 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 | % |
| Saturation,23°C | ISO 62 | 0.60 | % | |
| Shrinkage rate | MD | ISO 294-4 | 1.8 | % |
| TD | ISO 294-4 | 2.0 | % | |
| density | ISO 1183 | 1.27 | g/cm³ | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD,15Sec | ISO 868 | 74 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.