TPV Santoprene™ 121-70B230

109
  • Properties:
    Low friction coefficient
    UV resistance
    Recyclable materials
    Bondability
    Ozone resistance
  • Usages:
    Automotive sector
    Car exterior decoration
    Outdoor applications

Technical Data Sheet

hardnessTest ConditionTest MethodTest Result
ISO86865
elastomerTest ConditionTest MethodTest Result
Compression permanent deformation 3ISO81553 %
Tensile stress transverse flow rateASTMD4122.30 Mpa
Tensile stress transverse flow rateISO372.30 Mpa
Tensile strength - transverse flow rateASTMD4126.60 Mpa
tensile strength ISO376.60 Mpa
ASTMD412490 %
ISO37490 %
Compression permanent deformation 2ASTMD395B41 %
Compression permanent deformation 2ASTMD395B53 %
Compression permanent deformation 3ISO81541 %
agingTest ConditionTest MethodTest Result
The rate of change in tensile strength in airASTMD573-3.0 %
The rate of change in tensile strength in airISO188-3.0 %
ChangeinUltimateElongationAirASTMD573-10 %
ChangeinDurometerHardnessAirASTMD5732.0
ChangeinShoreHardnessinAirISO1882.0
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTMD746-52.0 °C
brittle temperatureISO812-52.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.