Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD1505 | 0.650 g/cm³ |
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Resin | 按重量计算的混合比:100 | ||
Hardener | 按重量计算的混合比:20 | ||
26 wk | |||
stripping time | 1400 min | ||
300 min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Compression Modulus | ASTMD695 | 2000 MPa | |
compressive strength | ASTMD695 | 35.9 MPa | |
shear strength | ASTMD732 | 13.1 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.