PA46 Stanyl® TS241B3 BK
46
- Properties:Thermal stability
- Usages:Automotive ApplicationsElectronic and electrical components
Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.22 g/cm³ | |
Water absorption rate | ISO 62 | 3.2 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 180-1A | 5.0 kJ/m² | |
tensile strength | ISO 527-2 | 185 Mpa | |
Tensile modulus | ISO 527-2 | 13000 Mpa | |
Flexural modulus | ISO 178 | 10500 Mpa |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melting temperature | ISO 3146 | 295 °C | |
Heat distortion temperature | ISO 75-1 | 290 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.