TP, Unspecified

TP, Unspecified Fluoroloy® A12

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.95 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessASTM D224060
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ASTM D170813.8 MPa
elongationBreakASTM D1708180 %
compressive strengthASTM D6956.89 MPa
coefficient of frictionASTM D37020.12
Heat distortion temperatureASTM D6213.00 %
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityASTM D44966.3E+18 ohms
Volume resistivityASTM D44968.2E+18 ohms·cm
dielectric strengthASTM D149>7.9 kV/mm
dielectric constantASTM D1502.40
Dissipation FactorASTM D1500.015
Thermal performanceTest ConditionTest MethodTest Result
thermal conductivity0.25 W/m/K
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.