Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1050 kg/m | |
Melt volume flow rate | ISO 1133 | 18.0 cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-1 | 2400 MPa | |
Tensile stress | ISO 527-1 | 47.0 MPa | |
Tensile strain | ISO 527-1 | 2.5 % | |
fracture strain | ISO 527-1 | 0.00 % | |
Charpy Notched Impact Strength | ISO 179/1eA | 19.0 KJ/m | |
ISO 179/1eA | 10.0 KJ/m | ||
ISO 179/1eU | 140 KJ/m | ||
ISO 179/1eU | 80.0 KJ/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Dielectric loss | IEC 60250 | 0.0060 | |
IEC 60250 | 0.0080 | ||
dielectric strength | IEC 60243-1 | 32 KV/mm | |
Volume resistivity | IEC 60093 | 1E+13 ohm.m | |
relative permittivity | IEC 60250 | 3.10 | |
IEC 60250 | 2.90 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | ISO 11359-1 | 0.000090 cm/cm℃ | |
Heat distortion temperature | ISO 75-1 | 100 ℃ | |
ISO 75-1 | 96.0 ℃ | ||
vicat | ISO 306 | 97.0 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.