Share
Add to compare

PUR-Ether//TDI LF 601D CHEMTURU USA

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

Uncured PropertiesTest ConditionTest MethodTest ResultTest Unit
Curing time100°C16hr
elastomerTest ConditionTest MethodTest ResultTest Unit
tensile strength100%StrainASTM D41225.5MPa
tensile strength200%StrainASTM D41232.4MPa
tensile strengthASTM D41248.3MPa
elongationBreakASTM D412290%
tear strength--2ASTM D624110kN/m
tear strengthSplitASTM D47020kN/m
Permanent compression deformation70°C,22hrASTM D395B28%
Shore hardnessASTM D263242%
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
compressive strength25%StrainASTM D69527.6MPa
compressive strength5%StrainASTM D6956.89MPa
compressive strength10%StrainASTM D69511.0MPa
compressive strength15%StrainASTM D69515.2MPa
compressive strength20%StrainASTM D69520.7MPa
thermosettingTest ConditionTest MethodTest ResultTest Unit
storage stability4.5min
stripping time20min
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
densityASTM D7921.16g/cm³
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreDASTM D224060to62
Shore hardness7.00
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.