Technical Data Sheet
performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Mass fraction of volatile matter,% ≤ | 150 | GB/T 6737-1997 热辊法 | |
Combined with the mass fraction of acrylonitrile,% | SH/T 1157-1997 | ||
300% tensile stress (145 ℃, 35min), MPa | SH/T 1611-2004 ASTM IRB No7 GB/T528-1998 | ||
Tensile strength (145 ℃, 35min), MPa ≥ | 24.4 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.