PBT 9K22220 FR1 4Plas
Properties:
Filler reinforcement material glass beads 20% filler processed by weight injection molding
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | reinforcement material | glass beads | 20% | filler processed by weight | injection molding |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179 | 5.0 | kJ/m² |
| 23°C | ISO 179/B | 6.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 35 | kJ/m² |
| 23°C | ISO 179/1eU | 40 | kJ/m² | |
| Impact strength of cantilever beam gap | -20°C | ISO 180/1A | 4.0 | kJ/m² |
| 23°C | ISO 180/1A | 5.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 | |
| 3.2mm | UL 94 | V-0 | ||
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 3.20 mm | UL 94 | V-0 | |
| 1.60 mm | UL 94 | V-0 | ||
| Hot filament ignition temperature | 2.00 mm | IEC 60695-2-13 | 960 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 5.0 | kJ/m² |
| Tensile modulus | 23°C | ISO 527-2/5 | 3750 | MPa |
| tensile strength | Break,23°C | ISO 527-2/5 | 60.0 | MPa |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 40 | kJ/m² |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 4.0 | kJ/m² |
| Tensile modulus | 23°C | ISO 527-2/5 | 3750 | MPa |
| tensile strength | Break, 23°C | ISO 527-2/5 | 60 | MPa |
| Tensile strain | Break, 23°C | ISO 527-2/5 | 4.0 | % |
| Charpy Notched Impact Strength | -30°C | ISO 179 | 5 | kJ/m² |
| 23°C | ISO 179/B | 6 | kJ/m² | |
| Tensile strain | Break,23°C | ISO 527-2/5 | 4.0 | % |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 35 | kJ/m² |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 170 | °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 70 | °C | |
| Melting temperature | ISO 11357 | 225 | °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 170 | °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 70.0 | °C | |
| Melting temperature | ISO 11357 | 225 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.57 | g/cm³ | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.13 | % |
| water content | ISO 960 | <1000 | ppm | |
| density | ISO 1183 | 1.57 | g/cm³ | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.13 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | 1E+14 | ohms | |
| Volume resistivity | IEC 60093 | 1E+16 | ohms·cm | |
| IEC 60093 | 1E+16 | ohms·cm | ||
| Surface resistivity | IEC 60093 | 1E+14 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.