plas
Log In

Rubber Silopren® LSR 4640 Momentive Performance Materials Inc.

0

Technical Data Sheet

Uncured PropertiesTest ConditionTest MethodTest Result
Color--3Translucent
Color--4Translucent
viscosity20°C3DIN 53018350 Pa·s
viscosity20°C4DIN 53018350 Pa·s
viscosityPot Life(20°C)DIN 530184300 min
elastomerTest ConditionTest MethodTest Result
tensile strengthDIN 535048.00 MPa
elongationBreakDIN 53504600 %
tear strengthASTM D62445.0 kN/m
Permanent compression deformation175°C,22hrDIN 5351725 %
thermosettingTest ConditionTest MethodTest Result
Thermosetting componentsPartA按重量计算的混合比:1.0
Thermosetting componentsPartB按重量计算的混合比:1.0
Thermosetting components后固化时间(200°C)4.0 hr
Physical propertiesTest ConditionTest MethodTest Result
densityDIN 534791.12 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreADIN 5350542
Supplementary InformationTest ConditionTest MethodTest Result
sulfurization175°C10.0 min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.