ASA Luran®S  S 757RE

466

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Water absorption rateISO621.7 %
Water absorption rateISO620.35 %
densityISO11831.07 g/cm³
Melt volume flow rateISO113325.0 cm3/10min
Shrinkage rateISO294-40.50to0.90 %
hardnessTest ConditionTest MethodTest Result
ISO2039-190.0 Mpa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO17912 kJ/m²
Impact strength of cantilever beam gapISO180/A4.0 kJ/m²
Impact strength of cantilever beam gapISO180/A11 kJ/m²
Charpy Notched Impact StrengthISO1793.0 kJ/m²
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO527-22400 Mpa
Tensile stressISO527-251.0 Mpa
Tensile strainISO527-23.3 %
TensileCreepModuleISO899-12200 Mpa
Tensile creep modulusISO899-11650 Mpa
Bending stressISO17875.0 Mpa
filmTest ConditionTest MethodTest Result
elongationISO527-38.0 %
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityIEC600931E+13 ohms
Volume resistivityIEC600931E+14 ohms·cm
dielectric constantIEC602503.40
Dissipation FactorIEC602500.010
Dissipation FactorIEC602500.025
Thermal performanceTest ConditionTest MethodTest Result
ISO75-2/B101 °C
ISO75-2/A96.0 °C
vicatISO306/A50105 °C
vicatISO306/B5097.0 °C
ISO11359-28.0E-5to1.1E-4 cm/cm/°C
thermal conductivityDIN526120.17 W/m/K
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.