| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 6.0 | kJ/m² |
| 23°C | ISO 180/1A | 8.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | Internal Method | V-2 | |
| 3.2mm | Internal Method | V-2 | ||
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 850 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Break | ISO 527-2 | 50.0 | MPa |
| Tensile strain | Break | ISO 527-2 | 5.0 | % |
| Bending modulus | ISO 178 | 3200 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | -- | ISO 306/A50 | 145 | °C |
| -- | ISO 306/B50 | 140 | °C | |
| BallPressureTest(125°C) | Pass | |||
| Hot deformation temperature | 1.8MPa,Annealed | ISO 75-2/A | 132 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.25 | g/cm³ | |
| melt mass-flow rate | 300°C/1.2kg | ISO 1133 | 11 | g/10min |
| Shrinkage rate | ISO 2577 | 0.20to0.50 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.