Rubber Shin-Etsu Elastomer SV-15000U Shin-Etsu Silicones of America
0
Technical Data Sheet
| Uncured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Curing time | 0.17 hr |
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 100%Strain | 1.39 MPa | |
| 9.16 MPa | |||
| elongation | Break | 440 % | |
| tear strength | 15.4 kN/m | ||
| Permanent compression deformation | 177°C,22hr | 9.0 % |
| thermosetting | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Post curing time | 200°C | 4.0 hr |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | 1.13 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | 51 |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| CureAgent | DBPH |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.