Share
Add to compare

PCTA MN621 EASTMAN USA

26

Form:Granules | Grade:Injection grade

Properties:
High mobilitytransparent
Typical Applications:
foodchip
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:food | chip
Properties:High mobility | transparent

Certificates

No Data...

Technical Data Sheet

optical performanceTest ConditionTest MethodTest ResultTest Unit
transmissivityTotalASTM D100391.0%
transmissivityRegularASTM D100389.0%
turbidityASTM D10030.30%
impact performanceTest ConditionTest MethodTest ResultTest Unit
Dart impact-40°C,EnergyatPeakLoadASTM D376348.0J
Dart impact23°C,EnergyatPeakLoadASTM D376345.0J
Multi axis Instrumented Impact Energy-40°C,能量to力量峰值ISO 6603-255.0J
Multi axis Instrumented Impact Energy23°C,能量to力量峰值ISO 6603-271.0J
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile strainBreak,23°CISO 527-2210%
Bending modulus23°CASTM D7901900Mpa
Bending modulus23°CISO 1781750Mpa
bending strength23°CISO 17864.0Mpa
bending strengthYield,23°CASTM D79067.0Mpa
tensile strengthYield,23°CASTM D63846.0Mpa
tensile strengthYield,23°CISO 527-247.0Mpa
tensile strengthBreak,23°CASTM D63853.0Mpa
tensile strengthBreak,23°CISO 527-249.0Mpa
elongationYield,23°CASTM D6385.0%
Tensile strainYield,23°CISO 527-24.0%
elongationBreak,23°CASTM D638310%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,UnannealedASTM D64873.0°C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B73.0°C
Hot deformation temperature1.8MPa,UnannealedASTM D64865.0°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A66.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateMD:3.20mmASTM D9550.20-0.60%
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardnessR-Sale,23°CASTM D785105
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.