TPE T-Blend® 5510N-PE Taiwan Synthetic Rubber
0
- Usages:Lining toothbrush handle household goods power other tools toys stationery sports equipment molded wrap soft handle
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tear strength | ASTM D624 | 21.6 kN/m | |
| elongation | Break | ASTM D412 | 350 % |
| tensile strength | Break | ASTM D412 | 3.14 MPa |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 180°C/5.0kg | ASTM D1238 | 1.0to9.0 g/10min |
| density | ASTM D792 | 1.07to1.11 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 54to58 |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Substrate | PP/PE |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.