PC EXL9330-WH6E276 SABIC INNOVATIVE NANSHA
137
Form:Granules
Properties:
Flame retardantTougheningUV resistance
Typical Applications:
foodThin walled productsCasters
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | food | Thin walled products | Casters |
| Properties: | Flame retardant | Toughening | UV resistance |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 60 | kJ/m² |
| 23°C | ISO 179/1eA | 75 | kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 | |
| 23°C | ISO 179/1eU | 无断裂 | ||
| Impact strength of cantilever beam gap | -50°C | ASTM D256 | 590 | J/m |
| -30°C | ASTM D256 | 680 | J/m | |
| 23°C | ASTM D256 | 800 | J/m | |
| 23°C8 | Internal Method | 1100 | J/m | |
| 23°C, 6.40 mm | ASTM D256 | 640 | J/m | |
| -30°C9 | ISO 180/1A | 55 | kJ/m² | |
| -30°C10 | ISO 180/4A | 65 | kJ/m² | |
| 23°C9 | ISO 180/1A | 70 | kJ/m² | |
| 23°C10 | ISO 180/4A | 80 | kJ/m² | |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | 无断裂 | |
| 23°C | ISO 180/1U | 无断裂 | ||
| Dart impact | 23°C, Total Energy | ASTM D3763 | 52.0 | J |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.5 mm | UL 94 | V-0 | |
| 3.0 mm | UL 94 | 5VA | ||
| Hot filament ignition temperature | 1.0 mm | IEC 60695-2-13 | 825 | °C |
| Burning wire flammability index | 1.0 mm | IEC 60695-2-12 | 960 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 35 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | --5,6 | ISO 178 | 85.0 | Mpa |
| Yield, 50.0 mm Span4 | ASTM D790 | 88.0 | Mpa | |
| Tensile modulus | --2 | ASTM D638 | 2100 | Mpa |
| -- | ISO 527-2/1 | 2100 | Mpa | |
| tensile strength | Yield3 | ASTM D638 | 58.0 | Mpa |
| Yield | ISO 527-2/50 | 55.0 | Mpa | |
| Break3 | ASTM D638 | 61.0 | Mpa | |
| Break | ISO 527-2/50 | 60.0 | Mpa | |
| elongation | Yield3 | ASTM D638 | 6.0 | % |
| Yield | ISO 527-2/50 | 6.0 | % | |
| Break3 | ASTM D638 | 130 | % | |
| Break | ISO 527-2/50 | 130 | % | |
| Bending modulus | 50.0 mm Span4 | ASTM D790 | 2060 | Mpa |
| --5 | ISO 178 | 2200 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Screw speed | 40 to 70 | rpm | ||
| Exhaust hole depth | 0.025 to 0.076 | mm | ||
| Back pressure | 0.300 to 0.700 | Mpa | ||
| Processing (melt) temperature | 295 to 315 | °C | ||
| Mold temperature | 70 to 95 | °C | ||
| drying temperature | 120 | °C | ||
| drying time | 3.0 to 4.0 | hr | ||
| Suggested maximum moisture content | 0.020 | % | ||
| Suggested injection volume | 40 to 60 | % | ||
| Temperature in the middle of the barrel | 280 to 305 | °C | ||
| Temperature at the rear of the barrel | 215 to 295 | °C | ||
| Temperature at the front of the material cylinder | 295 to 315 | °C | ||
| Spray nozzle temperature | 290 to 310 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45 MPa, Unannealed, 4.00 mm, 100 mm Span11 | ISO 75-2/Be | 135 | °C |
| 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 124 | °C | |
| 1.8 MPa, Unannealed, 4.00 mm, 100 mm Span11 | ISO 75-2/Ae | 124 | °C | |
| 1.8 MPa, Unannealed, 3.20 mm | ASTM D648 | 120 | °C | |
| Linear coefficient of thermal expansion | Flow : -40 to 40°C | ASTM E831 | 6.7E-5 | cm/cm/°C |
| Vicat softening temperature | -- | ASTM D152512 | 142 | °C |
| -- | ISO 306/B50 | 140 | °C | |
| Ball Pressure Test | 123 to 127°C | IEC 60695-10-2 | 通过 | |
| RTI | UL 746 | 120 | °C | |
| RTI Imp | UL 746 | 115 | °C | |
| Linear coefficient of thermal expansion | Across Flow : 23 to 80°C | ISO 11359-2 | 7.7E-5 | cm/cm/°C |
| RTI Elec | UL 746 | 125 | °C | |
| Linear coefficient of thermal expansion | Across Flow : -40 to 40°C | ASTM E831 | 6.7E-5 | cm/cm/°C |
| Flow : 23 to 80°C | ISO 11359-2 | 7.2E-5 | cm/cm/°C | |
| Hot deformation temperature | 0.45 MPa, Unannealed, 3.20 mm | ASTM D648 | 134 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | -- | ASTM D792 | 1.18 | g/cm³ |
| -- | ISO 1183 | 1.19 | g/cm³ | |
| melt mass-flow rate | 300°C/1.2 kg | ASTM D1238 | 10 | g/10 min |
| Melt Volume Flow Rate (MVR) | 300°C/1.2 kg | ISO 1133 | 9.00 | cm3/10min |
| Shrinkage rate | Flow : 3.20 mm | Internal Method | 0.40 - 0.80 | % |
| Across FlowFlow : 3.20 mm | Internal Method | 0.40 - 0.80 | % | |
| Water absorption rate | Saturation, 23°C | ISO 62 | 0.35 | % |
| Equilibrium, 23°C, 50% RH | ISO 62 | 0.15 | % | |
| Outdoor applicability | UL 746C | f1 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | > 1.0E+15 | ohms·cm | |
| Surface resistivity | IEC 60093 | > 1.0E+15 | ohms | |
| Dielectric constant | 1 MHz | ASTM D150 | 2.90 | |
| 50 kHz | ASTM D150 | 2.95 | ||
| 50 Hz | IEC 60250 | 2.60 | ||
| 1 MHz | IEC 60250 | 2.70 | ||
| 60 Hz | IEC 60250 | 2.60 | ||
| Dissipation factor | 50 Hz | ASTM D150 | 2.4E-3 | |
| 60 Hz | ASTM D150 | 2.4E-3 | ||
| 1 MHz | ASTM D150 | 8.5E-3 | ||
| 50 Hz | IEC 60250 | 1.0E-3 | ||
| 60 Hz | IEC 60250 | 1.0E-3 | ||
| Compared to the anti leakage trace index | UL 746 | PLC 3 | ||
| High arc combustion index | UL 746 | PLC 0 | ||
| Hot wire ignition | UL 746 | PLC 1 | ||
| Dielectric strength | 3.20 mm, in Oil | ASTM D149 | 17 | KV/mm |
| 3.20 mm, in Oil | IEC 60243-1 | 16 | KV/mm | |
| Dielectric constant | 60 Hz | ASTM D150 | 2.95 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | H 358/30 | ISO 2039-1 | 90.0 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.