TPU 3690AU Taiwan Bayer Youde
18
Form:Granules | Grade:Injection grade
Properties:
wear resistant
Typical Applications:
pipelinefilmFootwear
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | pipeline | film | Footwear |
| Properties: | wear resistant |
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Resilience | ISO 4662 | 29 | % | |
| Permanent compression deformation | 70°C, 24 hr6 | ISO 815 | 25 | % |
| 70°C, 24 hr4 | ISO 815 | 42 | % | |
| 23°C, 72 hr | ISO 815 | 21 | % | |
| tear strength | 23°C | ISO 34-1 | 95 | kN/m |
| squeeze out | Test Condition | Test Method | Test Result | Test Unit |
| Melt Temperature | 180 to 200 | °C | ||
| drying temperature | < 80 | °C | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Wear resistance | ISO 4649 | 25.0 | mm³ | |
| Tensile storage modulus | 60°C | ISO 6721 | 54.0 | Mpa |
| 20°C | ISO 6721 | 94.0 | Mpa | |
| -20°C | ISO 6721 | 940 | Mpa | |
| Tensile strain | Break, 23°C | DIN 53504 | 510 | % |
| tensile strength | 300% Strain, 23°C | DIN 53504 | 23.9 | Mpa |
| 100% Strain, 23°C | DIN 53504 | 10.0 | Mpa | |
| 50% Strain, 23°C | DIN 53504 | 8.00 | Mpa | |
| 10% Strain, 23°C | DIN 53504 | 3.50 | Mpa | |
| Break, 23°C | DIN 53504 | 60.2 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Mold temperature | 20 to 40 | °C | ||
| Processing (melt) temperature | 215 to 235 | °C | ||
| drying temperature | < 80 | °C | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | Shore D, 15 sec | ISO 8682 | 40 | |
| Shore A, 3 sec | ISO 8682 | 91 | ||
| Shore D, 1 Sec, 23°C | ISO 7619 | 40 | ||
| Shore A, 1 Sec, 23°C | ISO 7619 | 91 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.