Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.12 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore Hardness | Shore A | ASTMD2240 | 80 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-2 |
Limiting Oxygen Index | | ASTMD2863 | 25 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Taber Abrasion Resistance | | ASTMD3389 | 340 mg |
elastomer | Test Condition | Test Method | Test Result |
---|
Stretch permanent deformation | | ASTMD412 | 20 % |
tensile strength | | ASTMD412 | 46.0 MPa |
elongation | | ASTMD412 | 600 % |
compression set | | ASTMD395 | 20 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | DSC | -37.8 °C |
vicat | | ASTMD1525 | 90.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.