Technical Data Sheet
Cured Properties | Test Condition | Test Method | Test Result |
---|
Coverage-Cured | | | 0.672 cm³/g |
electric strength | | | 23 kV/mm |
| | | 3.70 |
Volume resistivity | | | 1E+13 ohms·cm |
Dissipation Factor | | | 0.030 |
Supporting hardness | | | 54到64 |
Supporting hardness | | | 60到68 |
tensile strength | | ASTMD412 | 4.48 MPa |
elongation | Break | ASTMD412 | 100 % |
tear strength | | ASTMD624 | 3.50 kN/m |
arc resistance | | | 125 sec |
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.49 g/cm³ |
Shrinkage Cured | | | 0.15 % |
thermosetting | Test Condition | Test Method | Test Result |
---|
| Resin | | 按重量计算的混合比:10按容量计算的混合比:100 |
| Hardener | | 按容量计算的混合比:15按重量计算的混合比:1.0 |
| Shelf Life | | 26 wk |
| | | 35000到45000 cP |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
colour | | | Beige |
| | | 65到75 Pa·s |
Curing Time | | | 16到18 hr |
STORAGE STABILITY | | | 60到120 min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | | 1E-03 cm/cm/°C |
thermal conductivity | | | 0.29 W/m/K |
ServiceTemperature-Cured | | | -51到218 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.