Technical Data Sheet
other | Test Condition | Test Method | Test Result |
---|
characteristic | | | 加工性能优良.稳定性高。 |
purpose | | | 热熔胶材料 |
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D-1238 | 60 g/10min |
Vinyl acetate content | | HCC Method | 40 % |
density | | ASTM D-1505 | 0.959 g/cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTM D-638 | 64 kg/cm |
Breaking point tensile strength | | ASTM D-638 | >1000 % |
Shore hardness | | ASTM D-2240 | 54 |
Physical properties | Test Condition | Test Method | Test Result |
---|
Vinyl acetate content | | | 40 % |
density | | ASTM D1505 | 0.959 g/cm² |
melt mass-flow rate | | ASTM D1238/ISO 1133 | 60 g/10min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ASTM D-1525 | <30 °C |
melting temperature | | ASTM D-3417 | 57 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.