PA12 MV1074 SA01 ARKEMA FRANCE
39
Form:Granules | Grade:Medical grade
Properties:
Low wear
Typical Applications:
Medical and nursing supplies
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Medical and nursing supplies |
| Properties: | Low wear |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | Internal Method | 1.502 | ||
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 | |
| 23°C | ISO 179/1eU | 无断裂 | ||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 19 | % | |
| squeeze out | Test Condition | Test Method | Test Result | Test Unit |
| drying temperature | 65 to 75 | °C | ||
| drying time | 4.0 to 6.0 | hr | ||
| Melt Temperature | 210 to 230 | °C | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2 | 97.0 | Mpa | |
| tensile strength | Break | ISO 527-2 | 30.0 | Mpa |
| 50% Strain | ISO 527-2 | 10.0 | Mpa | |
| Tensile strain | Break | ISO 527-2 | > 50 > 300 | % |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| drying temperature | 65 to 75 | °C | ||
| drying time | 4.0 to 6.0 | hr | ||
| Processing (melt) temperature | 200 to 270 | °C | ||
| Mold temperature | 25 to 60 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Glass transition temperature | ISO 11357-2 | -40.0 | °C | |
| Melting temperature | ISO 11357-3 | 158 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 1.4 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | -- | ohms | |
| Volume resistivity | IEC 60093 | 1.5E+11 | ohms·cm | |
| Dielectric strength | IEC 60243-1 | 5.0 | KV/mm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | Shore D, 15 Sec | ISO 868 | 40 | |
| film | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | MD : Break | ISO 527-3 | 32.0 | Mpa |
| TD : Break | ISO 527-3 | 34.0 | Mpa | |
| elongation | MD : Break | ISO 527-3 | 500 | % |
| TD : Break | ISO 527-3 | 700 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.