PPS PPS-hGR50 SICHUAN DEYANG
56
Form:Granules | Grade:Injection grade
Properties:
High temperature resistan
Typical Applications:
AerospaceAutomotive sectorElectrical appliancesElectronic fieldElectrical field
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Aerospace | Automotive sector | Electrical appliances | Electronic field | Electrical field |
| Properties: | High temperature resistan |
Certificates

Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| density | GB/T 1033-1986 | 1.68 | g/cm³ | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | GB/T 1040-1992 | 176 | Mpa | |
| compressive strength | GB/T 1041-1992 | 135 | Mpa | |
| Impact strength of cantilever beam gap | GB/T 1843-1996 | 13 | kJ/m² | |
| elongation | Break | GB/T 1040-1992 | 1.90 | % |
| Rockwell hardness | GB/T 9342-1988 | 111 | hr | |
| bending strength | GB/T 1042-1992 | 284.7 | Mpa | |
| Bending modulus | GB/T 1042-1992 | 1.63×104 | Mpa | |
| Elongation at Break | ASTM D638/ISO 527 | 1.63*100000 | % | |
| bending strength | ASTM D790/ISO 178 | 285 | kg/cm²(MPa)[Lb/in²] | |
| Rockwell hardness | ASTM D785 | 111 | ||
| tensile strength | ASTM D638/ISO 527 | 176 | kg/cm²(MPa)[Lb/in²] | |
| Elongation at Break | ASTM D638/ISO 527 | 1.9 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.80MPa | GB/T 1634-1979(1989) | 267 | °C |
| Melting temperature | GB/T 4608-1984 | 282 | °C | |
| Combustibility | 垂直法 | GB/T 2408-1996 | FV-0 | 级 |
| Melting temperature | 282 | ℃(℉) | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | GB/T 15585-1995 | 0.0025 | mm/mm | |
| density | ASTM D792/ISO 1183 | 1.68 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | GB/T 1410-1989 | 3.4×1014 | Ω.m | |
| Dielectric constant | 1MHz | GB/T 1409-1988 | 4 | |
| Dielectric strength | GB/T 1408.1-1999 | 19.1 | KV/mm | |
| Surface resistivity | GB/T 1410-1989 | 2.2×1015 | Ω |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.