Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.08 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | ASTMD2240 | 70 |
optical performance | Test Condition | Test Method | Test Result |
---|
refractive index | | ASTMD542 | 1.400 |
transmissivity | | ASTMD1003 | 85.0到95.0 % |
Haze ratio | | ASTMD1003 | <0.25 % |
Yellowness Index | | ASTMD1925 | <1.0 YI |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Break | ASTMD638 | 44.8 MPa |
tensile strength | | ASTMD638 | 3.10 MPa |
tensile strength | | ASTMD638 | 5.24 MPa |
tensile strength | | ASTMD638 | 12.2 MPa |
elongation | Break | ASTMD638 | 400 % |
elastomer | Test Condition | Test Method | Test Result |
---|
tear strength | | ASTMD624 | 52.5 kN/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | DSC | -57.0 °C |
| | ASTMD696 | 2E-04 cm/cm/°C |
TMA | | | 106 °C |
TMA | | | 83到130 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.