Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Resistance to environmental stress cracking | ASTMD1693 | <3.00 hr | |
density | ASTMD1505 | 0.965 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 8.0 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus- | Compression Molded | ASTMD638 | 931 MPa |
elongation | Break | ASTMD638 | 16 % |
Flexural modulus | ASTMD790 | 1720 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTMD256 | 48 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melting temperature | 118 °C | ||
Heat distortion temperature | ASTMD648 | 85.0 °C | |
ASTMD648 | 48.9 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.