Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | GB 3682 | 0.8 g/10min |
density | | GB 1033 | 0.942 g/cm³ |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | GB 1040 | 20.3 Mpa |
elongation | | GB 1040 | 640 % |
| | YD/T760-95 | 0/10 失效数 |
Other performance | Test Condition | Test Method | Test Result |
---|
colour | | YD/T760-95 | 本色 |
Immersion stability | | GB 1409 | 合格 |
Oxidation induction period (Cu cup) | | GB 2951.37 | 146 min |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Betweenness constant | | GB 1409 | 2.3 |
Dielectric loss factor | | GB 1409 | 1.54×10-4 |
Volume resistivity | | GB 1410 | 3.16×1014 Ω·M |
Thermal performance | Test Condition | Test Method | Test Result |
---|
low temperature brittleness | | GB 5470 | 0/10 失效数 |
Heat resistant stress cracking | | YD/T760-95 | 0/9 失效数 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.