IR SIBUR Synthetic Rubber IR SKI-3 NST Group I SIBUR RUSSIA
0
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 300%Strain | ASTM D3403 | >7.00 MPa |
| Yield | ASTM D3403 | >27.5 MPa | |
| elongation | Break | ASTM D3403 | >500 % |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Mooney viscosity | ML1+4,100°C | ASTM D1646 | 75to85 MU |
| Stearic Acid | Internal Method | 0.50to1.5 % | |
| ash content | ASTM D5667 | <0.50 % | |
| Volatile compounds | ASTM D5668 | <1.5 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.