电木粉 LONGLITE® T220NA
296
- Properties:High temperature resistanHigh impact resistancehigh strengthAging resistanceWeather resistancewear resistantHigh rigidity
- Usages:household electrical appliancesAutomotive Applications
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D570 | 0.1 % | |
Shrinkage rate | ASTM D955 | 0.005 m/m |
other | Test Condition | Test Method | Test Result |
---|---|---|---|
Electric trace resistance | 3 | ||
arc resistance | 4 | ||
Relative Heat Index (RTI) | 150 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ASTM D256 | 7 Kgf/cm | |
Impact strength of cantilever beam gap | ASTM D256 | 5.5 Kgf/cm | |
bending strength | ASTM D790 | 175 Mpa | |
tensile strength | ASTM D638 | 80 Mpa | |
compressive strength | ASTM D695 | 230 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+13 ohm-cm | |
dielectric strength | ASTM D149 | 14 KV/mm | |
insulation resistance | ASTM D257 | 1E+13 Ohm | |
ASTM D257 | 1E+12 Ohm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.