POM K300 KOLON KOREA
708
Form:Granules | Grade:Injection grade
Typical Applications:
currency
Product Description
Certificates(1)
Datasheet
Alternative(16)
Product Description
| Typical Applications: | currency |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 67 | J/m |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 7.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.8mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | ASTM D638 | 64.0 | Mpa | |
| Yield,23°C | ISO 527-2 | 65.0 | Mpa | |
| elongation | Yield,23°C | ASTM D638 | 60 | % |
| Tensile strain | Break,23°C | ISO 527-2 | 35 | % |
| Bending modulus | 23°C | ASTM D790 | 2500 | Mpa |
| 23°C | ISO 178 | 2700 | Mpa | |
| bending strength | 23°C | ISO 178 | 85.0 | Mpa |
| 23°C | ASTM D790 | 94.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 1.3E-04 | cm/cm/°C |
| Melting temperature | ASTM D3418 | 166 | °C | |
| ISO 11357-3 | 166 | °C | ||
| Vicat softening temperature | ASTM D1525 | 162 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 95.0 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 110 | °C | |
| 0.45MPa,Unannealed | ASTM D648 | 158 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.41 | g/cm³ | |
| ISO 1183 | 1.41 | g/cm³ | ||
| Water absorption rate | Equilibrium,23°C,60%RH | ASTM D570 | 0.22 | % |
| 23°C,24hr | ISO 62 | 0.59 | % | |
| Shrinkage rate | MD | ISO 294-4 | 2.3 | % |
| TD | ISO 294-4 | 2.2 | % | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 9.0 | g/10min |
| 190°C/2.16kg | ISO 1133 | 9.0 | g/10min | |
| Shrinkage rate | MD | ASTM D955 | 2.0 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | ASTM D150 | 3.70 | ||
| Dielectric strength | IEC 60243-1 | 19 | KV/mm | |
| ASTM D149 | 19 | KV/mm | ||
| Volume resistivity | IEC 60093 | 1E+14 | ohms·cm | |
| ASTM D257 | 1E+14 | ohms·cm | ||
| Surface resistivity | IEC 60093 | 1E+16 | ohms | |
| ASTM D257 | 1E+16 | ohms | ||
| Dissipation factor | 1MHz | ASTM D150 | 6E-03 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Scale | ISO 2039-2 | 93 | |
| M-Scale | ASTM D785 | 80 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.