PC 1803R SABIC INNOVATIVE SHANGHAI
141
Form:Granules
Properties:
high viscosityHigh temperature resistanenhanceThermal stabilityFlame retardant
Typical Applications:
Automotive sectorLaptop caseElectronic fieldElectrical field
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Automotive sector | Laptop case | Electronic field | Electrical field |
| Properties: | high viscosity | High temperature resistan | enhance | Thermal stability | Flame retardant |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | ASTMD542 | 1.586 | ||
| transmissivity | 2540μm | ASTM D1003 | 88.0to90.0 | % |
| turbidity | 2540μm | ASTM D1003 | <0.80 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| -30°C | ISO 180/1U | 无断裂 | ||
| 23°C | ASTMD4812 | 无断裂 | ||
| ISO 180/1A | 70 | kJ/m² | ||
| -30°C | ISO 180/1A | 12 | kJ/m² | |
| 23°C | ASTM D256 | 700 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.60mm | UL 94 | V-2 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| crack | ISO 527-2/50 | >70 | % | |
| ASTM D638 | >70 | % | ||
| yield | ISO 527-2/50 | 6.0 | % | |
| ASTM D638 | 6.0 | % | ||
| ISO 527-2/50 | 63.0 | Mpa | ||
| ASTM D638 | 63.0 | Mpa | ||
| --2 | ASTM D638 | 2350 | Mpa | |
| Yield, 50.0mm span | ASTM D790 | 90.0 | Mpa | |
| --8 | ISO 178 | 90.0 | Mpa | |
| --7 | ISO 178 | 2300 | Mpa | |
| 50.0mm span | ASTM D790 | 2300 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass | |
| -40 to 95 ° C | ASTME831 | 7E-05 | cm/cm/°C | |
| 23 to 80 ° C | ISO 11359-2 | 7E-05 | cm/cm/°C | |
| thermal conductivity | DENKA Method | 0.20 | W/m/K | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTMD792 | 1.20 | g/cm³ | |
| Balance, 23 ° C | ASTM D570 | 0.35 | % | |
| Saturation, 23 ° C | ISO 62 | 0.35 | % | |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 | % |
| MD:--1 | Internal Method | 0.50-0.70 | % | |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 17.0 | cm3/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | ASTMD257 | >1.0E+15 | ohms·cm | |
| Dielectric strength | 1.60mm | ASTM D2863 | 27 | KV/mm |
| Dielectric constant | 60Hz | ASTMD150 | 3.00 | |
| 1MHz | ASTMD150 | 3.00 | ||
| Dissipation factor | 60Hz | ASTMD150 | 1E-03 | |
| 1MHz | ASTMD150 | 0.010 | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Hardness (Rockwell R) | ISO 2039-2 | 120 | ||
| ASTM D785 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.