Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
StyreneContent | | | 40 % |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
density | | | 1.12 g/cm³ |
| | | 0.40 Pa·s |
GelTime | | | 9.0 min |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 39 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
GeltoPeak | | | 10.0 min |
PeakExotherm | | | 187 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 3380 MPa |
tensile strength | | ASTMD638 | 85.5 MPa |
elongation | Break | ASTMD638 | 4.0 % |
Flexural modulus | | ASTMD790 | 3930 MPa |
bending strength | | ASTMD790 | 141 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD4812 | 220 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 91.7 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.