Fluorelastomer Boda BDP-H7802

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.98 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224083
elastomerTest ConditionTest MethodTest Result
tensile strengthYieldASTMD41227.2 MPa
elongationBreakASTMD412280 %
compression setASTMD39523 %
agingTest ConditionTest MethodTest Result
volume changeASTMD4712.0 %
Change rate of tensile strength in airASTMD573-11 %
Change rate of ultimate elongation in airASTMD573-12 %
The rate of change in hardness of an air hardness testerASTMD5731.0
Change rate of tensile strengthASTMD471-5.0 %
Change rate of ultimate elongationASTMD471-8.0 %
The rate of change in hardness of a hardness testerASTMD471-2.0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.