Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD1505 | 0.923 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 0.80 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTMD2457 | 60 |
transparency | | ASTMD1746 | 45.0 |
Haze ratio | | ASTMD1003 | 8.5 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| | ASTMD1894 | 0.45 |
film | Test Condition | Test Method | Test Result |
---|
Film thickness - tested | | | 50 µm |
Available film thickness | | | 30to200µm |
tensile strength | | ASTMD882 | 16.0 Mpa |
tensile strength | | ASTMD882 | 12.0 Mpa |
tensile strength | | ASTMD882 | 24.0 Mpa |
tensile strength | | ASTMD882 | 22.0 Mpa |
elongation | | ASTMD882 | 500 % |
elongation | | ASTMD882 | 600 % |
Falling hammer impact 2 | | ASTMD1709B | 150 g |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ASTMD1525 | 95.0 °C |
Crystallization peak temperature | | ASTME794 | 112 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.