TPE 2190

0
  • Properties:
    Injection molding reference process: temperature at the rear of the barrel
    140-160 ℃
    holding pressure
    30-120MPa
    temperature at the middle of the barrel
    150-170 ℃
    mold temperature
    20-50 ℃
    temperature at the front of the barrel
    160-180 ℃
    holding time
    15-75S nozzle temperature
    170-190 ℃
    screw speed
    20-100r
    min
    injection pressure
    40-150MPa
    injection speed?

Technical Data Sheet

Basic performanceTest ConditionTest MethodTest Result
relative density1.30 g/cm
Mechanical propertiesTest ConditionTest MethodTest Result
tear strength62.0 kN/m
tensile strength 16.0 MPa
Shore hardness90 A
Elongation330 %
stretching strength8.0 MPa
Other performanceTest ConditionTest MethodTest Result
Retention rate of elongation at break88 %
Volume change of fuel B0 %
Tensile strength retention rate108 %
permanent set51 %
Constant tensile strength retention rate129 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.