TPV Alloy Elastoprene 90A-4000

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7920.960 g/cm³
hardnessTest ConditionTest MethodTest Result
ASTMD224090
ASTMD224087
Supplementary InformationTest ConditionTest MethodTest Result
OzoneResistanceASTMD1149Excellent
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD4127.60 MPa
tensile strengthASTMD41214.2 MPa
elongationASTMD412590 %
tear strengthASTMD62449.0 kN/m
compression setASTMD39555 %
compression setASTMD39563 %
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTMD746-55.0 °C
melting temperature159 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.