PC Resblend ABS/PC Polimarky Spolka Jawna
0
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1A | 15to20 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 2000to2500 MPa | |
| tensile strength | ISO 527-2 | 45.0to55.0 MPa | |
| Tensile strain | Break | ISO 527-2 | 5.0to15 % |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ISO 1183 | 1.07to1.18 g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.